The design of interfaces, coupled with suitable joining materials and joining technologies, is a key parameter in component manufacturing and surface pre-treatments are crucial steps for the production of robust and reliable bonds. In this work, plasma pre-treatments on SiC and Si3N4 are studied and discussed. The pre-treated joined samples have shown a higher mechanical strength than the reference value (lapped surfaces) and the increased adhesion at the ceramic/adhesive interface has led to cohesive failure of the adhesive
A plasma pre-treatment to improve adhesion on SiC and Si3N4 ceramics
Casalegno V.; Ferraris M.; Perero S.; Suess M.; Wilhelmi C.; Pedroni M.; Vassallo E.; Salvo M.
ID | 422835 |
---|---|
DOI | 10.1016/j.matlet.2020.127855 |
PRODUCT TYPE | Journal Article |
LAST UPDATE | 2022-02-04T15:32:10Z |